The extraction of metal ore in the poor leads us to look for techniques and methods to extract a good amount of it (metal) low cost without passing the gangue in the solution. For this purpose, to determine leaching parameters seen to recover the metal in a low grade ore, we proceeded to test leaching guidelines heap ore preceded by size analysis and chemical different slices to determine the working parameters that can give satisfactory results. After these analyzes guidance, we opted for crushing the ore to determine the correct job settings for a good recovery of the metal contained in the ore poor and know the slice for perfect contact between the etching solution and ore for metal recovery. During testing after leaching, we noticed that when we respect the following parameters: a constant acid concentration of 70 g / l, a time of 64 hours, a particle size of 1,700 micron; we dissolved a good amount of metals or a yield ranging between 37.9 to 74.9% when the particle size of the ore pass 9423-850 micron. However, leaching of the composite sample of the same ore, gives a neighbor leach performance to which is recorded with the fine ore 70.8%.
Author Keywords: yield, leaching, Ore, copper-cobaltifere, granulometry.
Patrick MBWEB KATSHIL1
1 Commissariat Général à l’Energie Atomique, Ministère de la Recherche Scientifique, Lubumbashi, RD Congo
Original language: French
Copyright © 2017 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Abstract
The extraction of metal ore in the poor leads us to look for techniques and methods to extract a good amount of it (metal) low cost without passing the gangue in the solution. For this purpose, to determine leaching parameters seen to recover the metal in a low grade ore, we proceeded to test leaching guidelines heap ore preceded by size analysis and chemical different slices to determine the working parameters that can give satisfactory results. After these analyzes guidance, we opted for crushing the ore to determine the correct job settings for a good recovery of the metal contained in the ore poor and know the slice for perfect contact between the etching solution and ore for metal recovery. During testing after leaching, we noticed that when we respect the following parameters: a constant acid concentration of 70 g / l, a time of 64 hours, a particle size of 1,700 micron; we dissolved a good amount of metals or a yield ranging between 37.9 to 74.9% when the particle size of the ore pass 9423-850 micron. However, leaching of the composite sample of the same ore, gives a neighbor leach performance to which is recorded with the fine ore 70.8%.
Author Keywords: yield, leaching, Ore, copper-cobaltifere, granulometry.
Abstract: (french)
L’extraction du métal dans le minerai pauvre nous amène à chercher des techniques et méthodes permettant à extraire une bonne quantité de ce dernier (le métal) à faible coût sans faire passer la gangue dans la solution. A cet effet, pour déterminer les paramètres de lixiviation en vu de récupérer le métal dans un minerai pauvre, nous avons procédé aux essais d’orientations de lixiviations en tas du minerai précédé par des analyses granulométriques et chimiques des différentes tranches en vue de déterminer les paramètres de travail pouvant donner des résultats satisfaisant. Après ces analyses d’orientations, nous avons opté pour le broyage du minerai, afin de déterminer les bons paramètres de travail pour une bonne récupération du métal contenu dans le minerai pauvre et connaitre la tranche permettant un contact parfait entre la solution d’attaque et le minerai pour la récupération du métal. Lors des analyses après lixiviation, nous avons remarqué que, lorsque nous respectons les paramètres ci-après : une concentration en acide constante de 70 g/l, un temps de 64 heures, une granulométrie de 1700 micron ; nous mettons en solution une bonne quantité des métaux soit un rendement qui varie entre 37,9 à 74,9 % quand la granulométrie du minerai passe de 9423 à 850 micron. Cependant, la lixiviation de l’échantillon composite du même minerai, donne un rendement de lixiviation voisin à celui que l’on enregistre avec les minerais fins, soit 70,8%.
Author Keywords: rendement, Lixiviation, Minerai, cupro-cobaltifère, granulométrie.
How to Cite this Article
Patrick MBWEB KATSHIL, “Etude de la lixiviation en tas du minerai cupro-cobaltifère dans les mines de la Province du Katanga en République Démocratique du Congo,” International Journal of Innovation and Applied Studies, vol. 20, no. 2, pp. 575–588, May 2017.