[ Valorisation de l’attapulgite de Pout comme inhibiteur de corrosion du fer à béton Fe500-3 dans la solution interstitielle du béton ]
Volume 24, Issue 4, November 2018, Pages 1603–1613
Malang Bodian1, Dame Keinde2, Alpha Ousmane Touré3, Prince Momar Gueye4, and Modou Fall5
1 Département de Chimie, Laboratoire de Chimie Physique Organique et d’Analyses Environnementales, Faculté des Sciences et Techniques, Université Cheikh Anta Diop, Dakar, Senegal
2 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
3 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
4 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
5 Département de Chimie, Laboratoire de Chimie Physique Organique et d’Analyses Environnementales, Faculté des Sciences et Techniques, Université Cheikh Anta Diop, Dakar, Senegal
Original language: French
Copyright © 2018 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
The behavior of Fe500-3 iron was studied in the interstitial solution of mortar concrete, formulated from sand, cement, water, admixtures and in the presence of a clay (attapulgite) added as corrosion inhibitor. Indeed, in most cases in Senegal, mixing water and sand used in concrete formulations for buildings are subject to no treatment. The study solution was synthesized from these concretes at the 3rd, 7th and 28th day of wet cure. Fe500-3 iron corrosion tests in the interstitial concrete solution were carried out by monitoring the free corrosion potential, Tafel polarization curves and electrochemical impedance spectroscopy measurement. The protective power of attapulgite was also evaluated by electrochemical methods with different levels of inhibitor (0 to 20%). The measurements reveal a probable attack of Fe500-3 iron at the 3rd and 7th day of cure in the absence of inhibitor and the protective effect of the interstitial solution of the concretes without inhibitor at the 28th day of cure by the formation of a protective layer on the iron surface. The results also showed the corrosion inhibition effect of the clay on the 3rd and 7th day of cure by the formation of a protective film on the surface of the metal. The layer thickness increases with the content of the clay. A maximum average inhibitory efficiency of about 87.8% was obtained at the 7th day of cure at the 20% clay content.
Author Keywords: attapulgite, corrosion, inhibition, clay, concrete.
Volume 24, Issue 4, November 2018, Pages 1603–1613
Malang Bodian1, Dame Keinde2, Alpha Ousmane Touré3, Prince Momar Gueye4, and Modou Fall5
1 Département de Chimie, Laboratoire de Chimie Physique Organique et d’Analyses Environnementales, Faculté des Sciences et Techniques, Université Cheikh Anta Diop, Dakar, Senegal
2 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
3 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
4 Département de Génie Civil, Laboratoire de Matériaux de génie Civil (LMGC), Ecole Supérieure Polytechnique de Dakar, Université Cheikh Anta Diop, Dakar, Senegal
5 Département de Chimie, Laboratoire de Chimie Physique Organique et d’Analyses Environnementales, Faculté des Sciences et Techniques, Université Cheikh Anta Diop, Dakar, Senegal
Original language: French
Copyright © 2018 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Abstract
The behavior of Fe500-3 iron was studied in the interstitial solution of mortar concrete, formulated from sand, cement, water, admixtures and in the presence of a clay (attapulgite) added as corrosion inhibitor. Indeed, in most cases in Senegal, mixing water and sand used in concrete formulations for buildings are subject to no treatment. The study solution was synthesized from these concretes at the 3rd, 7th and 28th day of wet cure. Fe500-3 iron corrosion tests in the interstitial concrete solution were carried out by monitoring the free corrosion potential, Tafel polarization curves and electrochemical impedance spectroscopy measurement. The protective power of attapulgite was also evaluated by electrochemical methods with different levels of inhibitor (0 to 20%). The measurements reveal a probable attack of Fe500-3 iron at the 3rd and 7th day of cure in the absence of inhibitor and the protective effect of the interstitial solution of the concretes without inhibitor at the 28th day of cure by the formation of a protective layer on the iron surface. The results also showed the corrosion inhibition effect of the clay on the 3rd and 7th day of cure by the formation of a protective film on the surface of the metal. The layer thickness increases with the content of the clay. A maximum average inhibitory efficiency of about 87.8% was obtained at the 7th day of cure at the 20% clay content.
Author Keywords: attapulgite, corrosion, inhibition, clay, concrete.
Abstract: (french)
Le comportement du fer Fe500-3 a été étudié dans la solution interstitielle du béton à mortier formulé à partir du sable, du ciment, de l’eau, d’un adjuvant et en présence d’une argile (attapulgite) ajoutée comme inhibiteur de corrosion. En effet, dans la plupart des cas au Sénégal, l’eau de gâchage ainsi que le sable utilisés dans les formulations du béton pour les constructions ne sont soumis à aucun traitement. La solution d’étude a été synthétisée à partir de ces bétons au 3ème, 7ème et 28éme jour de cure humide. Les tests de corrosion du fer Fe500-3 dans la solution interstitielle des bétons ont été réalisés par le suivi du potentiel de corrosion libre, les courbes de polarisation de Tafel et par des mesures de spectroscopie d’impédance électrochimique. Le pouvoir protecteur de l’attapulgite vis-à-vis du Fer Fe500-3 a également été évalué par les méthodes électrochimiques à différentes teneurs en inhibiteur (0 à 20%). Les mesures révèlent une attaque probable du fer Fe500-3 aux 3ème et au 7ème jours de cure en absence d’inhibiteur et l’effet protecteur de la solution interstitielle des bétons sans inhibiteur au 28éme jour de cure par la formation d’une couche protectrice à la surface du fer. Les résultats ont également montré l’effet inhibiteur de la corrosion de l’argile aux 3ème et 7ème jours de cure par la formation d’un film protecteur à la surface du métal. L’épaisseur de la couche augmente avec la teneur de l’argile. Une efficacité inhibitrice moyenne maximale d’environ 87,8% a été obtenue au 7ème jour de cure à la teneur de 20% en argile.
Author Keywords: attapulgite, corrosion, inhibition, argile, béton.
How to Cite this Article
Malang Bodian, Dame Keinde, Alpha Ousmane Touré, Prince Momar Gueye, and Modou Fall, “Valorization of Pout attapulgite as corrosion inhibitor for Fe500-3 concrete reinforcing iron in the interstitial solution of concrete,” International Journal of Innovation and Applied Studies, vol. 24, no. 4, pp. 1603–1613, November 2018.