Twitter
|
Facebook
|
Google+
|
VKontakte
|
LinkedIn
|
Viadeo
|
English
|
Français
|
Español
|
العربية
|
 
International Journal of Innovation and Applied Studies
ISSN: 2028-9324     CODEN: IJIABO     OCLC Number: 828807274     ZDB-ID: 2703985-7
 
 
Thursday 21 November 2024

About IJIAS

News

Submission

Downloads

Archives

Custom Search

Contact

  • Contact us
  • Newsletter:

Connect with IJIAS

  Now IJIAS is indexed in EBSCO, ResearchGate, ProQuest, Chemical Abstracts Service, Index Copernicus, IET Inspec Direct, Ulrichs Web, Google Scholar, CAS Abstracts, J-Gate, UDL Library, CiteSeerX, WorldCat, Scirus, Research Bible and getCited, etc.  
 
 
 

Preliminary tests for recovering by bottled cyanidation from combined lateritic and clayey ores samples of the gold-bearing province of Yaouré in central Côte d'Ivoire (West Africa)


[ Tests préliminaires de récupération par cyanuration en bouteilles d'échantillons combinés de minerais latéritique et argileux de la province aurifère du Yaouré dans le Centre de la Côte d'Ivoire (Afrique de l'Ouest) ]

Volume 2, Issue 2, February 2013, Pages 180–188

 Preliminary tests for recovering by bottled cyanidation from combined lateritic and clayey ores samples of the gold-bearing province of Yaouré in central Côte d'Ivoire (West Africa)

Paul Tonga TIEMOKO1 and Gbele Ouattara2

1 Département des Sciences de la Terre et des Ressources Minières (STeRMi)/Laboratoire du Génie Civil, des Géosciences et Sciences géographiques/Institut National Polytechnique Félix Houphouët-Boigny, Yamoussoukro, Côte d'Ivoire
2 Département des Sciences de la Terre et des Ressources Minières (STeRMi), Laboratoire du Génie Civil, des Géosciences et Sciences géographiques, Institut National Polytechnique Félix Houphouët-Boigny, Yamoussoukro, Côte d'Ivoire

Original language: French

Copyright © 2013 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

Abstract


The Yaoure gold deposit (Central Ivory Coast, West Africa) is composed of several types of ores: quartz vein, sulphide facies (45-50 m in depth), oxidized facies (35-45 m in depth) and, on the surface, a clayey zone. Therefore some physical features like permeability are essential in the heap leaching method. Taken separately, the ore associated with the clay show some recovery problems, when the humidity level is more than 12 to 15%. For this cause, the Department of science and mining resources of INP-HB has study the blending method thus to face that problem. It's consisting of mixing the clayey ore with different other types of ore proportionally to obtain a heterogeneous ore and increase its permeability thus. A leaching test has been achieved on six samples (blended clayey and lateritic ores) to determine the maximum recovery and the optimum consumption in reagents (NaCN and CaO). The tests results permit to obtain the best figure with 96.63% of reconstituted quantity recovery with reagents consumption of 1.41 kg/t in NaCN and 0.45 kg/t in CaO. In addition, some in column leaching tests must be done often to simulate the leaching in heap with the aim of determining some technical, physical and economic parameters to improve the process and therefore to increase the recovery.

Author Keywords: Lateritic and clayey ores, Cyanidation in bottle, Gold recovery rate, Yaour.


Abstract: (french)


Le gisement d'or de la province aurifère du Yaouré (Centre de la Côte d'Ivoire) est constitué de plusieurs types de minerais dont, du quartz filonien, un faciès sulfuré en profondeur (45-50 m), un faciès oxydé de mi-profondeur (35-45 m) et, plus en surface, un faciès argileux. Ces minerais sont donc de perméabilités différentes, propriété essentielle pour la cyanuration. Pris individuellement, le minerai argileux pose des difficultés de cyanuration liées à son imperméabilité lorsque l'humidité est supérieure à 12 – 15%. Ce qui a emmené le Département de recherche et de formation en Sciences de la Terre de l'INP-HB à étudier la méthode du blending qui consiste à combiner les différents types de minerais en roche avec le minerai argileux, afin de le rendre hétérogène et augmenter ainsi sa perméabilité. Des essais de lixiviation en bouteilles ont été réalisés sur six échantillons combinés de minerais argileux et latéritique pour déterminer le taux de récupération maximum et la consommation optimum en réactifs (NaCN et CaO). Les tests réalisés sur une densité de pulpe à 50% de solides montrent que le meilleur résultat obtenu au cours de ces essais indique une récupération de 96,63% de l'or en calculant par rapport aux quantités reconstituées, avec une consommation en réactifs de 1,41 kg/t pour le NaCN et 0,45 kg/t pour le CaO. Pour la suite de l'étude, des essais de lixiviation en colonne doivent se faire pour simuler la lixiviation en tas et en déterminer les paramètres économiques.

Author Keywords: Minerais latéritique et argileux, Cyanuration en bouteilles, Taux de récupération de l'or, Province aurifère du Yaouré, Centre de la Côte d'Ivoire, Afrique de l'Ouest.


How to Cite this Article


Paul Tonga TIEMOKO and Gbele Ouattara, “Preliminary tests for recovering by bottled cyanidation from combined lateritic and clayey ores samples of the gold-bearing province of Yaouré in central Côte d'Ivoire (West Africa),” International Journal of Innovation and Applied Studies, vol. 2, no. 2, pp. 180–188, February 2013.