[ Amélioration des caractéristiques mécaniques des briques comprimées par ajout de cendres de bois ]
Volume 38, Issue 1, November 2022, Pages 197–204
K. A. Kouassi1, L. M. Thieblesson2, A. S. Djomo3, and A. C. Djohore4
1 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
2 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
3 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
4 Laboratoire des Politiques Energétiques et Environnemental, Institut de Recherche sur les Energies Nouvelles, Universite Nangui Abrogoua d’Abobo-Adjamé 02 BP 801 Abidjan 02, Côte d’Ivoire
Original language: French
Copyright © 2022 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
The purpose of this study is to design compressed earth bricks and evaluate the mechanical characteristics in the dry and wet state. To achieve this, bricks were made by adding ash and cement to clay sand. Different materials were elaborated in dry and wet state. The formulation of the materials is as follows: 05% of cement for 25% of ash for the first material, 05% of cement and 05% of ash for the second type and 03% of cement for 03% of ash for the last. All the bricks were tested in compression, at 14 days for some and 14 days plus 3 days of immersion in water for others. The different results obtained at the end of the different laboratory performance tests give compressive strengths of 3.28 MPa for the first type of formulation; 2.18 MPa for the second type and 2.06 MPa for the third type of formulation at 14 days in a dry state. In the wet state, the compressive strength is 2.05 MPa for the first type of mix; 1.09 MPa for the second type and 1.40 MPa for the third type of mix at 14 days and three days of immersion with the same cement and ash dosages. The optimum strength is obtained for dosages of 05% cement for 25% wood ash.
Author Keywords: Bingerville, BTC, materials, compressive strength, ash.
Volume 38, Issue 1, November 2022, Pages 197–204
K. A. Kouassi1, L. M. Thieblesson2, A. S. Djomo3, and A. C. Djohore4
1 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
2 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
3 UFR Environnement, Université Jean Lorougnon GUEDE de Daloa, B.P 150 Daloa, Côte d’Ivoire
4 Laboratoire des Politiques Energétiques et Environnemental, Institut de Recherche sur les Energies Nouvelles, Universite Nangui Abrogoua d’Abobo-Adjamé 02 BP 801 Abidjan 02, Côte d’Ivoire
Original language: French
Copyright © 2022 ISSR Journals. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Abstract
The purpose of this study is to design compressed earth bricks and evaluate the mechanical characteristics in the dry and wet state. To achieve this, bricks were made by adding ash and cement to clay sand. Different materials were elaborated in dry and wet state. The formulation of the materials is as follows: 05% of cement for 25% of ash for the first material, 05% of cement and 05% of ash for the second type and 03% of cement for 03% of ash for the last. All the bricks were tested in compression, at 14 days for some and 14 days plus 3 days of immersion in water for others. The different results obtained at the end of the different laboratory performance tests give compressive strengths of 3.28 MPa for the first type of formulation; 2.18 MPa for the second type and 2.06 MPa for the third type of formulation at 14 days in a dry state. In the wet state, the compressive strength is 2.05 MPa for the first type of mix; 1.09 MPa for the second type and 1.40 MPa for the third type of mix at 14 days and three days of immersion with the same cement and ash dosages. The optimum strength is obtained for dosages of 05% cement for 25% wood ash.
Author Keywords: Bingerville, BTC, materials, compressive strength, ash.
Abstract: (french)
Cette étude a pour but de concevoir des briques de terre comprimée et évaluer les caractéristiques mécaniques à l’état sec et humide. Pour y parvenir, des briques ont été réalisées par ajout de cendre et de ciment au sable argileux. Différents matériaux ont été élaborés à l’état sec et humide. La formulation des matériaux est la suivante: 05% de ciment pour 25% de cendre pour le premier matériau, 05% de ciment et 05% de cendre pour le deuxième type et 03% de ciment pour 03% de cendre pour le dernier. Toutes les briques ont été testées à la compression, à 14 jours pour certains et 14 jours plus 3 jours d’immersion dans l’eau pour d’autres. Les différents résultats obtenus à la fin des différents tests de performances en laboratoire donnent des résistances à la compression de 3,28 MPa pour le premier type de formulation; de 2,18 MPa pour le deuxième type et 2,06 MPa pour le troisième type de formulation à 14 jours à l’état sec. A l’état humide, la résistance à la compression est de 2,05 MPa pour le premier type de formulation; de 1,09 MPa pour le deuxième type et de 1,40MPa pour le troisième type de formulation à 14 jours et trois jours d’immersion avec les mêmes dosages en ciment et en cendre. La résistance optimale est obtenue pour des dosages à 05% de ciment pour 25% de cendre de bois.
Author Keywords: Bingerville, BTC, matériaux, résistance à la compression, cendre.
How to Cite this Article
K. A. Kouassi, L. M. Thieblesson, A. S. Djomo, and A. C. Djohore, “Improvement of the mechanical characteristics of compressed bricks by adding wood ash,” International Journal of Innovation and Applied Studies, vol. 38, no. 1, pp. 197–204, November 2022.